Hastelloy S nickel round bar, UNS N06635 nickel plate

HASTELLOY S alloy (UNS N06635) is a nickel-base, high-temperature alloy with a unique combination of properties. It has excellent thermal stability, low thermal expansion and excellent oxidation resistance to 2000°F (1093°C). In addition, the alloy has good high-temperature and thermal fatigue strength. S alloy retains its strength and ductility after aging at temperatures of 800 to 1600°F (427 to 871°C). S alloy was developed for applications involving severely cyclical heating conditions where components must be capable of retaining their strength, ductility, and metallurgical integrity after long-time exposure. It is used extensively as seal rings in gas turbine engines where its low thermal expansion coefficients is also important.

Products Details

Elements Content (%)
Nickel, Ni 67
Chromium, Cr 14.5 - 17
Molybdenum, Mo 14 - 16.5
Iron, Fe 3
Cobalt, Co 2
Tungsten, W 1
Copper, Cu 0.35
Manganese, Mn 0.30 - 1.0
Silicon, Si 0.20 - 0.75
Aluminum, Al 0.10 - 0.50
Carbon, C 0.020
Phosphorous, P 0.020
Boron, B 0.015
Sulfur, S 0.015
Lanthanum, La 0.010 - 0.10
▪ AMS 5711 ▪ AMS 5838 ▪ AMS 5873Hastelloy S has good machining characteristics. Tooling is required to avoid work hardening and chatter.Hastelloy S can be formed using conventional methods.Hastelloy S is welded using metal inert gas and tungsten inert gas welding methods.Hastelloy S is heat treated by annealing at 1066°C (1950°F) followed by cooling in air.Hastelloy S is forged at 872 to 1149°C (1600 to 2100°F).Hastelloy S can be hot worked at 872 to 1149°C (1600 to 2100°F).Hastelloy S can be easily cold worked.Hastelloy S is annealed at 1066°C (1950°F) followed by cooling in air.Hastelloy S is aged at 538 to 872°C (1000 to 1600°F) in order to restores its ductility and strength.Hastelloy S can be hardened by cold working.Hastelloy S is used in gas turbines.

Contact us

Please feel free to give your inquiry in the form below We will reply you in 24 hours