WASPALOY is a nickel based age hardenable alloy that possesses high temperature strength while still having a good corrosion resistance, especially to oxidation. WASPALOY can be used at temperatures up to 650°C (1200°F) which is critical rotating applications. WASPALOY is used in gas turbine engine components, missile systems, shafts, spacers, seals, rings, casings, fasteners and many other uses in engine hardware, airframe assemblies. Waspaloy 25 is a nickel- base alloy with excellent high-temperature strength and good resistance to oxidation at a temperature up to 1800° F. This superalloy has higher stability and strength ranges than those available for alloy 718. Waspaloy 25™ can be heat treated through a three-step process: solution treatment, stabilization, and age-hardening.

Products Details

Cr 18.0-21.0 B 0.003-0.01
Zr 0.02-0.12 Al 1.2-1.6
Ti 2.75-3.25 Mo 3.5-5.0
Co 12.0-15.0 Cu 0.5 max
Fe 2.0 max S 0.03 max
Si 0.75 max Mn 1.0 max
C 0.02-0.1 max P 0.03 max
Ni Balance  
1.Rod, Bar, Wire and Forging Stock 2.ASTM B 637, ISO 9723, ISO 9724, ISO 9725, AMS 5704, AMS 5706, AMS 5707, AMS 5708, AMS 5709, AMS 5828, MAM 5706, AECMA PrEN 2193, AECMA PrEN 2194, AECMA PrEN 2406, AECMA PrEN 2958, AECMA PrEN 2959, AECMA PrEN 2960, AECMA PrEN 3220. 3.Plate, Sheet and Strip 4.AMS 5544, AECMA PrEN 2195 5.Other 6.UNS N07001, W. Nr 2.4654, MSRR 7192
Material Condition Thickness Temp. Tensile Strength ksi Yield Strength ksi Elongation in 4D Hardness HRC
Sheet Sol Treated, Stabilization + Precipitation HT 0-0.020" Room 170 110 15 34-44
Sheet Sol Treated, Stabilization + Precipitation HT 0-0.020" 1000°F 145 100 13  
Sheet Sol Treated, Stabilization + Precipitation HT over 0.020" Room 175 115 20 34-44
Sheet Sol Treated, Stabilization + Precipitation HT over 0.020" 1000°F 150 105 15  
Properties as per AMS 5708 type 2 (capable of AMS 5709) Heat Treatment is as follows Solution Treat 1900 - 1975°F / 1-4 hours and Air Cool Resulting hardness not higher than 302HB Stabilization Heat Treatment Heat to 1550°F / 4 hrs and Air Cool Precipitation Heat Treatment Heat to 1400°F / 16 hrs and Air Cool Resulting hardness 32-42 HRCHeat Treatment is as follows Annealing 1975°F / 30 mins and Air Cool Solution Heat Treatment 1825°F / 2hrs and Air Cool Stabilization Heat Treatment 1550°F /4hrs and Air Cool Precipitation Heat Treatment 1400°F / 16 hrs and Air Cool